Gold Embrittlement Mitigation: Understanding the New J-STD-001 Requirements


Reading time ( words)

A significant change to the soldering assembly specifications is outlined in the recently released "F" version of the J-STD-001, Requirements for Soldered Electrical and Electronic Assemblies (July 2014) for gold-plated components. With the advent of more information from studies on the behavior of how much gold can impact the mechanical structure of the solder joint, the "washing away" of gold has become more important.

Gold is widely used in electronic package finish designs in order to enhance solderability and wire bondability. A thick, pure gold finish can be used to enhance wire bondability, but can be too thick for soldering, causing solder joint embrittlement. It does not oxidize very readily, melts at relatively low temperature, and dissolves rapidly in the soldering process. However, too much remnant gold in the solder joint can weaken the integrity of the interconnection.

If the gold dissolution is excessive during the solder alloy’s liquid phase formation, then the composition, mechanical properties and durability of the resulting joint alloy can change, compared with the original solder alloy. As the finished electronic assemblies heat up and cool down, or when exposed to stresses, the gold in the solder joint can weaken or embrittle it and fail. Given the above understandings, solder joint embrittlement is defined as a change of solder joint durability due to dissolution and/or reaction with a finish such as gold and/or palladium.

The changes are expressed in tin-based solders by the appearance of AuSn4 intermetallic compounds from gold finishes. The compounds can occur in the bulk of the solder joint, at the finish interface or in both locations. The compounds are brittle in comparison with the soft solder alloy. As a result, the ability of the joint to be robust when subjected to mechanical strains is reduced.

Limiting these localized weaknesses and maintaining a reliable solder joint is the reason, along with the corresponding testing to verify this, behind the J-STD specification change.

Changes in the J-STD-001 Specification

With the advent of the new version of IPC JSTD-001, the governing the assembly of printed circuit boards, changes to the procurement and preparation of gold plated parts for the military and aerospace markets has taken a new turn.

The following significant changes were made to the specification:

1. Gold embrittlement mitigation (gold washing), which when not done, was a process indicator for class 2 assemblies in "E" is now a defect if NOT done in "F"

2. All through-hole leads required to be hand-soldered regardless of gold thickness need to be "washed" (and hence are a reliability concern

3. A new warning that gold embrittled solder terminations can be present when the solder volume is low (i.e., very small components) or when the dwell time is not sufficient in the soldering process

Read The Full Article Here

Editor's Note: This article originally appeared in the October 2015 issue of SMT Magazine.

Share




Suggested Items

Real Time with … IPC APEX EXPO 2023: Mycronic Extends Reach

01/11/2023 | Nolan Johnson, I-Connect007
Clemens Jargon, senior vice president of High Flex at Mycronic, shares his thoughts about the company’s performance in 2022 (it was a strong year), plans for the new year (turnkey solutions), and what visitors to the Mycronic booth at the show can expect to see in the company’s state-of-the-art Iris™ 3D AOI vision technology.

Five-Star Reflow Recipes: Q&A With Rob Rowland

12/28/2022 | Andy Shaughnessy, I-Connect007
In this Q&A, Rob Rowland, director of engineering at Axiom Electronics, discusses his new IPC APEX EXPO Professional Development course, “Reflow Profiling Simplified,” on how to create a standardized methodology to accurately generate new reflow soldering profiles. Rob explains, “In this class, I’ll explain how I approached this work to help others develop similar methodologies for creating their own reflow soldering profiles. My presentation also includes the basic reflow profile recipes I have been using for the past 20 years.”

Essemtec: Manufacturing Moves In-house

12/28/2022 | Pete Starkey, I-Connect007
Pete Starkey talks with Kevin Domancich at Essemtec at electronica 2022 about the company integration within Nano Dimension and how the two companies have pioneered an exciting new end-to-end manufacturing solution that helps customers speed up production, cut costs, and keep their proprietary materials secure. In a world where time to market has become a priority consideration, this universal system has the potential to revolutionize the industry.



Copyright © 2023 I-Connect007 | IPC Publishing Group Inc. All rights reserved.